首页> 外国专利> METHODS OF IDENTIFYING A CERAMIC MATERIAL EXHIBITING AN ELECTRIC FIELD INDUCED STRAIN DERIVED FROM A REVERSIBLE PHASE TRANSITION, METHODS OF PREPARATION AND CERAMIC MATERIALS OBTAINABLE THEREFROM

METHODS OF IDENTIFYING A CERAMIC MATERIAL EXHIBITING AN ELECTRIC FIELD INDUCED STRAIN DERIVED FROM A REVERSIBLE PHASE TRANSITION, METHODS OF PREPARATION AND CERAMIC MATERIALS OBTAINABLE THEREFROM

机译:识别由可逆相变产生的电场诱发的应变的陶瓷材料的方法,制备方法和可从中获得的陶瓷材料

摘要

The present invention relates to a method for identifying a solid solution ceramic material of a plurality of perovskite compounds which exhibits an electric field induced strain derived from a reversible phase transition, as well as a method for making such ceramic materials and ceramic materials obtainable therefrom. In particular, the present invention is directed to a method of identifying a solid solution ceramic material of at least three perovskite compounds which exhibits an electric field induced strain derived from a reversible phase transition; said method comprising the steps of: i) determining a molar ratio of at least one tetragonal perovskite compound to at least one non-tetragonal perovskite compound which, when combined to form a solid solution, provides a ceramic material comprising a major portion of a tetragonal phase having an axial ratio c/a of greater than 1.005 to 1.04; and ii) determining a molar ratio of at least one additional non-tetragonal perovskite compound to the combination of perovskite compounds from step i) at the determined molar ratio which, when combined to form a solid solution, provides a ceramic material comprising a major portion of a pseudo-cubic phase having an axial ratio c/a of from 0.995 to 1.005 and/or a rhombohedral angle of 90±0.5 degrees.
机译:本发明涉及一种鉴定多种钙钛矿化合物的固溶体陶瓷材料的方法,该固溶体陶瓷材料表现出源自可逆相变的电场感应应变,并且涉及一种制备这种陶瓷材料和由其获得的陶瓷材料的方法。特别地,本发明涉及一种鉴定至少三种钙钛矿化合物的固溶体陶瓷材料的方法,所述固溶体陶瓷材料表现出源自可逆相变的电场感应应变。所述方法包括以下步骤:i)确定至少一种四方钙钛矿化合物与至少一种非四方钙钛矿化合物的摩尔比,当组合形成固溶体时,其提供包含大部分四方钙钛矿的陶瓷材料。轴向比c / a大于1.005至1.04的相; ii)以确定的摩尔比确定至少一种另外的非四方钙钛矿化合物与来自步骤i)的钙钛矿化合物的组合的摩尔比,当组合形成固溶体时,提供包含主要部分的陶瓷材料轴立方比c / a为0.995至1.005和/或菱形角为90±0.5度的假立方相。

著录项

  • 公开/公告号EP3577091A1

    专利类型

  • 公开/公告日2019-12-11

    原文格式PDF

  • 申请/专利权人 XAAR TECHNOLOGY LIMITED;

    申请/专利号EP20180704065

  • 申请日2018-02-02

  • 分类号C04B35/475;H01L41/187;C04B35/462;C04B35/465;C04B35/468;

  • 国家 EP

  • 入库时间 2022-08-21 11:40:02

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号