A glass has a basic soda-lime-silica glass portion, and a colorant portion including total iron as Fe2O3 selected from the group of total iron as Fe2O3 in the range of greater than zero to 0.02 weight percent; total iron as Fe2O3 in the range of greater than 0.02 weight percent to less than 0.10 weight percent and total iron as Fe2O3 in the range of 0.10 to 2.00 weight percent; redox ratio in the range of 0.2 to 0.6, and tin and/or tin compounds, e.g. SnO2 greater than 0.000 to 5.0 weight percent. In one embodiment of the invention, the glass has a tin side and an opposite air side, wherein the tin side of the glass is supported on a molten tin bath during forming of the glass. The tin concentration at the tin side of the glass is greater than, less than, or equal to the tin concentration in "body portion" of the glass. The "body portion" of the glass extending from the air side of the glass toward the tin side and terminating short of the tin side of the glass.
机译:玻璃具有碱性钠钙硅玻璃部分和着色剂部分,该着色剂部分包括作为总铁的元素的Fe 2 O 3 。 > 2 O 3 的范围大于零到0.02重量百分比;总铁为Fe 2 O 3 的范围大于0.02重量%至小于0.10重量%,总铁为Fe 2 O 3 的重量百分比在0.10到2.00之间;氧化还原比在0.2到0.6的范围内,锡和/或锡化合物例如SnO 2 大于0.000至5.0重量百分比。在本发明的一个实施例中,玻璃具有锡面和相对的空气面,其中在玻璃形成期间,玻璃的锡面被支撑在熔融锡浴上。玻璃的锡侧的锡浓度大于,小于或等于玻璃的“主体部分”中的锡浓度。玻璃的“主体部分”从玻璃的空气侧向锡侧延伸并且终止于玻璃的锡侧的短端。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号