首页> 外国专利> Method for producing maleic anhydride-modified vinyl chloride resin composition

Method for producing maleic anhydride-modified vinyl chloride resin composition

机译:马来酸酐改性的氯乙烯树脂组合物的制造方法

摘要

PROBLEM TO BE SOLVED: To obtain a maleic anhydride-modified polyvinyl chloride resin composition which is not colored and is modified with maleic anhydride at a high addition rate while suppressing thermal decomposition of polyvinyl chloride and adhesion to a metal. Provide a manufacturing method for. SOLUTION: Polyvinyl chloride, 0.5 to 20 parts by mass of a heat stabilizer with respect to 100 parts by mass of the polyvinyl chloride, and 1 to 30 parts by mass of anhydrous maleine with respect to 100 parts by mass of the polyvinyl chloride. Melt the acid, 0.05 to 5 parts by mass of an organic peroxide with respect to 100 parts by mass of the polyvinyl chloride, and 0.5 to 10 parts by mass of an outer lubricant with respect to 100 parts by mass of the polyvinyl chloride. The content of the compound having at least one functional group selected from the group consisting of a thiol group and a hydroxyl group as the heat stabilizer, which comprises kneading, is 0, based on 100 parts by mass of the polyvinyl chloride. A method for producing a maleic anhydride-modified polyvinyl chloride resin composition, which is less than 01 ppm. [Selection diagram] None
机译:解决的问题:获得不着色且以高添加率用马来酸酐改性的马来酸酐改性的聚氯乙烯树脂组合物,同时抑制聚氯乙烯的热分解和对金属的粘附。提供一种制造方法。溶液:相对于100质量份的聚氯乙烯,聚氯乙烯,相对于100质量份的聚氯乙烯为0.5至20质量份的热稳定剂和相对于100质量份的聚氯乙烯为1至30质量份的无水马来酸。相对于100质量份的聚氯乙烯,使酸,0.05至5质量份的有机过氧化物和相对于100质量份的聚氯乙烯的0.5至10质量份的外部润滑剂熔融。基于100质量份的聚氯乙烯,具有捏合的具有至少一个选自硫醇基和羟基的官能团作为热稳定剂的化合物的含量为0。小于01ppm的马来酸酐改性的聚氯乙烯树脂组合物的制造方法。 [选择图]无

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号