首页> 外国专利> Heat-resistant chlorine-containing crosslinked resin molded article and method for producing the same, silane masterbatch and masterbatch mixture, and heat-resistant product

Heat-resistant chlorine-containing crosslinked resin molded article and method for producing the same, silane masterbatch and masterbatch mixture, and heat-resistant product

机译:耐热含氯交联树脂成型品及其制备方法,硅烷母料和母料混合物以及耐热产品

摘要

For a base resin containing chlorinated polyethylene, polyvinyl chloride, and a plasticizer, an organic peroxide, an inorganic filler, and a silane coupling agent, at a specific ratio, which is equal to or higher than the decomposition temperature of the organic peroxide. Step (a) of melt-mixing at a temperature, step (b) of molding after mixing the silane master batch obtained in step (a) and the silanol condensation catalyst, and step (b) of forming the molded article. (C) cross-linking by contact with moisture, and in step (a), 5-55% by mass of a plasticizer in 100% by mass of a base resin used at the time of reaction with the silane coupling agent. A method for producing a heat-resistant chlorine-containing crosslinked resin molded article, a heat-resistant chlorine-containing crosslinked resin molded article produced thereby, a silane masterbatch and a mixture thereof, and a heat-resistant product.
机译:对于包含氯化聚乙烯,聚氯乙烯和增塑剂的基础树脂,有机过氧化物,无机填料和硅烷偶联剂的特定比例等于或高于有机过氧化物的分解温度。步骤(a)在一定温度下熔融混合,步骤(b)在将步骤(a)中获得的硅烷母料和硅烷醇缩合催化剂混合之后成型,并且步骤(b)形成成型品。 (C)通过与水分接触而交联,在步骤(a)中,相对于硅烷偶联剂反应时使用的基础树脂100质量%,增塑剂为5〜55质量%。耐热性含氯交联树脂成型体的制造方法,由此制造的耐热性含氯交联树脂成型体,硅烷母料及其混合物,以及耐热性产品。

著录项

  • 公开/公告号JPWO2018180690A1

    专利类型

  • 公开/公告日2020-02-06

    原文格式PDF

  • 申请/专利权人 古河電気工業株式会社;

    申请/专利号JP20190509340

  • 发明设计人 西口 雅己;松村 有史;

    申请日2018-03-19

  • 分类号C08J3/20;C08J3/24;C08C19/25;C08F259/02;C08L51;C08K3/013;C08K5/12;

  • 国家 JP

  • 入库时间 2022-08-21 11:31:51