The purpose of the notification is to obtain bone scaffolding on the basis of flouoroapatete and polymer. This means that for the aqueous suspension of ss-1,3-glucan (kurdlan),containing an 8-to-20 advantageous 10-14-weight Kurdlan fraction of 100-weight water, the porous granules of phosphate-calcium fluorine ceramics of the size 0,1-1-1 mm in the quantity of 3 to 9,5 advantageous 4-to 8-weight granules are added to 1-weight Kurdlan and mixed until uniform mass is obtained, then the precursor obtained is placed in forms and heating. Bone scaffolding containing thermally polymerised beta-1,3-glucan (Kurdlan) is also covered by the notification,pre-moistened, the aqueous suspension of Kurdlan contains from 8 to 20 parts of the weight of Kurdlan in 100 parts of the weight of the water and phosphate calcium fluorine ceramics in the form of granules of the size 0,1 -1 mm, with proportions of the solids being three to 9,5 parts of the weight of the granules in one part of the weight of the Kurdlan.
机译:该通知的目的是获得基于氟代磷酸根和聚合物的骨支架。这意味着对于含有100重量份水的8到20有利的10-14重量份Kurdlan分数的ss-1,3-葡聚糖(kurdlan)水性悬浮液,磷酸钙氟陶瓷的多孔颗粒将尺寸为1-1-1毫米,数量为3至9.5的4至8重量的有利颗粒添加至1重量的库德兰并混合直至获得均匀的质量,然后将获得的前体以一定形式放置和加热。该通知还涵盖了含有热聚合的β-1,3-葡聚糖(Kurdlan)的骨脚手架,预先润湿,Kurdlan的水悬浮液在100重量份的Kurdlan中含有8至20重量份的Kurdlan。尺寸为0.1 -1毫米的颗粒形式的水和磷酸盐钙氟陶瓷,其中固体的比例为颗粒重量的三至9.5份,占Kurdlan重量的一部分。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号