The invention discloses a self-heating inorganic adhesive. The self-heating inorganic adhesive comprises two components and concretely comprises an inorganic adhesive semi-finished product and a quicklime gelatin capsule in a weight ratio of (40-60): (10-25). The inorganic adhesive semi-finished product is prepared from 30-60 parts by weight of water, 20-30 parts by weight of aluminum hydroxide, 20-35 parts by weight of phosphoric acid, 10-20 parts by weight of calcium sulfate, 4-10 parts by weight of fly ash, 3-5 parts by weight of calcium carbonate, 2-4 parts by weight cooked glutinous riceflour and 0.3-0.7 parts by weight of curcumin. The invention also discloses a preparation method of the self-heating inorganic adhesive. Through use of the cooked glutinous rice flour as the initial adhesive, the initial viscosity of the adhesive is effectively increased. Through use of the inorganic adhesive in the production of agricultural and forestry residual fiber (planing) boards, the problems of loosing in the board blank transportation and loading and unloading are solved. Compared with other initial adhesives, the cooked glutinous rice flour has obvious price advantages.
机译:本发明公开了一种自热无机胶粘剂。自加热的无机粘合剂包括两种成分,具体地包括重量比为(40-60):(10-25)的无机粘合剂半成品和生石灰明胶胶囊。无机粘合剂半成品由30-60重量份的水,20-30重量份的氢氧化铝,20-35重量份的磷酸,10-20重量份的硫酸钙,4制备。 -10重量份的粉煤灰,3-5重量份的碳酸钙,2-4重量份的糯米粉和0.3-0.7重量份的姜黄素。本发明还公开了一种自热无机胶的制备方法。通过使用蒸煮的糯米粉作为初始粘合剂,粘合剂的初始粘度被有效地提高。通过在农林残余纤维(刨花)板生产中使用无机胶粘剂,解决了板坯运输,装卸中松动的问题。与其他初始粘合剂相比,煮熟的糯米粉具有明显的价格优势。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号