The present invention relates to a wool-like polyester filament and a preparation method therefor. The method comprises: first, uniformly mixing terephthalic acid, 1,4-butanediol, a fluorine-containing diacid, hexanediol having a tertiary butyl side group, and 2,5,6,6-tetramethyl-2,5,-heptanediol; then sequentially performing an esterification reaction and a polycondensation reaction to prepare a modified polyester; preparing a modified polyester POY filament from a modified polyester melt according to a POY process; finally, preparing a modified polyester DTY filament, i.e., the wool-like polyester filament, from the modified polyester POY filament according to a DTY process. The dye uptake of a prepared product is 90.32-93.27% under the temperature of 100°C, and a K/S value is 22.15-23.42; after being placed at the temperature of 25°C and the relative humidity of 65% for 60 months, the intrinsic viscosity of the product decreases by 17-20%. By means of the preparation method of the present invention, the present invention is low in cost and simple in process; the prepared product has an excellent dyeing property and a fast natural degradation rate, and has great application prospects.
机译:羊毛状聚酯长丝及其制备方法本发明涉及一种羊毛状聚酯长丝及其制备方法。该方法包括:首先,将对苯二甲酸,1,4-丁二醇,含氟二酸,具有叔丁基侧基的己二醇和2,5,6,6-四甲基-2,5,-庚二醇均匀地混合;然后依次进行酯化反应和缩聚反应以制备改性聚酯。根据POY工艺由改性聚酯熔体制备改性聚酯POY长丝;最后,根据DTY方法,由改性聚酯POY长丝制备改性聚酯DTY长丝,即羊毛状聚酯长丝。制备产物在100℃温度下的染料吸收率为90.32-93.27%,K / S值为22.15-23.42。在25°C的温度和65%的相对湿度下放置60个月后,产品的特性粘度降低17-20%。通过本发明的制备方法,本发明成本低廉,工艺简单。所制备的产品具有优异的染色性能和快速的自然降解速率,具有广阔的应用前景。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号