A stainless steel composite plate for use in petroleum and natural gas delivery pipelines, comprising a base material and a coating material, the coating material being metallurgically coated onto the base material, the coating material being austenitic stainless steel, and the chemical composition of the base material by weight percentage being: C: 0.03%-0.09%, Si: 0.2%-0.4%, Mn: 1.00%-1.70%, P≤0.02%, S≤0.01%, Alt: 0.015%-0.050%, Nb: 0.020%-0.090%, V≤0.05%, Ti: 0.006%-0.030%, Cr: 0.10%-0.30%, Ni≤0.30%, Mo≤0.10%, Cu≤0.30%, B≤0.001%, and the remainder being Fe and a small amount of unavoidable impurities; and a preparation method for the stainless steel composite plate for use in petroleum and natural gas delivery pipelines, the preparation method being simple and easy to implement and low cost; the prepared composite plate has good corrosion resistance and strong toughness, a straighter composite interface, more uniform coating thickness, and better surface quality, and can be directly used without needing annealing heat treatment.
机译:一种用于石油和天然气输送管道的不锈钢复合板,包括基材和涂层材料,该涂层材料以冶金方式涂覆在该基材上,该涂层材料为奥氏体不锈钢,以及该基材的化学组成材料的重量百分比为:C:0.03%-0.09%,Si:0.2%-0.4%,Mn:1.00%-1.70%,P≤0.02%,S≤0.01%,Alt:0.015%-0.050%,Nb: 0.020%-0.090%,V≤0.05%,Ti:0.006%-0.030%,Cr:0.10%-0.30%,Ni≤0.30%,Mo≤0.10%,Cu≤0.30%,B≤0.001%,其余是铁和少量不可避免的杂质;一种用于石油天然气输送管道的不锈钢复合板的制备方法,该方法简单易行,成本低廉。制备的复合板具有良好的耐蚀性和韧性,复合界面更直,涂层厚度更均匀,表面质量更好,无需退火热处理即可直接使用。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号