SUPERHYDROPHOBIC-SUPEROLEOPHILIC NICKEL FOAMS AND METHOD FOR PREPARING SAME

机译:超疏水-超亲油性镍泡沫及其制备方法

摘要

The present invention relates to a superhydrophobic-superoleophilic nickel foam coated with a coating mixture comprising polytetrafluoroethylene (PTFE) and hydrophobic fumed silica, as well as a method for preparing the same. The method for preparing a superhydrophobic-superoleophilic nickel foam comprises steps of: preparing slurry; providing a nickel foam to be coated with the slurry; and dip coating the nickel foam with the slurry. According to the present invention, the nickel foam may be coated with a coating mixture comprising polytetrafluoroethylene (PTFE) and hydrophobic fumed silica to prepare a superhydrophobic-superoleophilic nickel foam, thus having an effect of facilitating a separation between water and oil.;COPYRIGHT KIPO 2020
机译:本发明涉及用包含聚四氟乙烯(PTFE)和疏水性气相二氧化硅的涂料混合物涂覆的超疏水-超亲油性镍泡沫及其制备方法。该超疏水-超亲油性镍泡沫的制备方法包括以下步骤:制备浆料;制备浆料。提供泡沫镍,以用浆料涂覆;然后用浆料浸涂泡沫镍。根据本发明,可以用包含聚四氟乙烯(PTFE)和疏水性热解法二氧化硅的涂料混合物涂覆泡沫镍,以制备超疏水-超亲油性镍泡沫,从而具有促进水和油之间分离的作用。 2020年

著录项

  • 公开/公告号KR20200036492A

    专利类型

  • 公开/公告日2020-04-07

    原文格式PDF

  • 申请/专利号KR20180116189

  • 发明设计人 KO JANG MYOUNKR;

    申请日2018-09-28

  • 分类号C09K3/18;B05D1/18;B05D3/02;B05D5;B05D7/14;B05D7/24;C09D127/16;C09D127/18;C09D7/62;C09K3/32;

  • 国家 KR

  • 入库时间 2022-08-21 11:07:23

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号