Reduction method of hematite

机译:赤铁矿的还原方法

摘要

The present invention comprises the steps of preparing raw pellets by mixing hematite (Fe 2 O 3 ) with water (H 2 O), drying the raw pellets to remove moisture, dried raw pellets, coal and comprising the step of causing the hematite (Fe 2 O 3) a reduction reaction by heating the mixture of step and the dried raw pellets, the coal and the calcium carbonate (CaCO 3) of mixing a calcium carbonate (CaCO 3), wherein by a reduction reaction is reduced to the hematite (Fe 2 O 3) is at least one selected from the group consisting of FeO and Fe 3 O 4 iron oxide, tight the hematite according to the above reduction reaction yirueojim (Fe 2 O 3) It relates to a method for reducing hematite, characterized in that the sulfur (Sulfur) component contained in the reduction. According to the present invention, desulfurization and reduction may be possible at the same time.
机译:本发明包括以下步骤:通过将赤铁矿(Fe 2 O 3 )与水(H 2 O)混合,干燥粗粒来制备粗粒料。去除湿气的原料丸,干燥的原料丸,煤,并且包括通过加热步骤和混合物的混合物使赤铁矿(Fe 2 O 3)还原的步骤。干燥的原始颗粒,煤和碳酸钙(CaCO 3)混合的碳酸钙(CaCO 3),其中通过还原反应还原成赤铁矿(Fe 2 O 3)是选自FeO和Fe 3 O 4 氧化铁中的至少一种,根据上述还原反应yueueojim(Fe 2 O 3)紧缩赤铁矿。一种还原赤铁矿的方法,其特征在于,其中所含的硫(硫)成分在减少。根据本发明,脱硫和还原可以同时进行。

著录项

  • 公开/公告号KR20200076882A

    专利类型

  • 公开/公告日2020-06-30

    原文格式PDF

  • 申请/专利权人 한국세라믹기술원;

    申请/专利号KR20180165831

  • 发明设计人 노동규;추용식;김경석;제현모;

    申请日2018-12-20

  • 分类号C04B41/80;C04B35/26;C04B41;

  • 国家 KR

  • 入库时间 2022-08-21 11:06:36

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号