The present invention provides a polyethylene-based resin composition for an expandable laminate having excellent height and appearance of a foam cell (foaming layer) having a sufficient height and appearance by heating, and having excellent microwave suitability. The present invention is a polyethylene-based resin composition for a foamable laminate that forms a polyethylene-based resin layer (I) for foaming on at least one side of a paper substrate, wherein the polyethylene-based resin composition for a foamable laminate is (a-1) to ( and a polyethylene resin (A) satisfying the properties of a-3). (a-1) MFR is 6 g / 10 min or more but less than 20 g / 10 min; (a-2) The density is 0.920 to 0.930 g / cm 3 ; (a-3) In the elution curve obtained by temperature rise elution fractionation (TREF) with orthodichlorobenzene, the ratio of the eluate at an elution temperature of 70 ° C or higher is 47 to 83% by weight.
机译:本发明提供了一种用于发泡性层压体的聚乙烯基树脂组合物,该组合物具有优异的高度和外观,并且通过加热具有足够的高度和外观的泡沫单元(发泡层)具有优异的微波适用性。本发明是一种用于可发泡层压材料的聚乙烯基树脂组合物,其在纸基材的至少一侧上形成用于发泡的聚乙烯基树脂层(I),其中,所述用于发泡性层压材料的聚乙烯基树脂组合物为( a-1)〜(a)和满足a-3)的性质的聚乙烯树脂(A)。 (a-1)MFR为6克/ 10分钟或以上,但少于20克/ 10分钟; (a-2)密度为0.920至0.930 g / cm 3 ; (a-3)在用邻二氯苯进行升温洗脱分级分离(TREF)得到的洗脱曲线中,洗脱温度为70℃以上的洗脱液的比例为47〜83重量%。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号