首页> 外国专利> Modified asphalt mixture

Modified asphalt mixture

机译:改性沥青混合料

摘要

The modified asphalt mixture according to the present invention (i) has a diameter of 10 to 900 nm with respect to 100 parts by weight of asphalt, and a hollow part 12 is formed in the center of the body 11 along the longitudinal direction, 2 to 8 parts by weight of carbon nano-hollow fiber 10 in which micropores 13 for communicating the outer surface of the body 11 and the hollow part 12 are irregularly formed, and (iii) linear styrene-butadiene -It is characterized in that 10 to 30 parts by weight of a urethane polymer, 30 to 80 parts by weight of polyethylene wax, and 5 to 10 parts by weight of a modifier mixed with 10 to 50 parts by weight of process oil are mixed with respect to 100 parts by weight of styrene synthetic rubber. The present invention improves the strength and frictional durability while reducing the plastic change of the asphalt pavement, and can significantly lower the mixing temperature of the aggregate and asphalt during the manufacture of the asphalt mixture and the compaction temperature during the construction of the asphalt pavement, thereby shortening the construction period. It reduces energy consumption.
机译:相对于100重量份的沥青,本发明的改性沥青混合料(i)的直径为10至900nm,并且在主体11的中央沿长度方向2形成有中空部12。 8至8重量份的碳纳米空心纤维10,其中不规则地形成了用于连通主体11的外表面和中空部分12的微孔13,和(iii)线性苯乙烯-丁二烯-其特征在于,相对于100重量份的聚氨酯树脂,将30重量份的聚氨酯聚合物,30-80重量份的聚乙烯蜡和5-10重量份的改性剂与10-50重量份的加工油混合。苯乙烯合成橡胶。本发明在降低沥青路面的塑性变化的同时提高了强度和摩擦耐久性,并且可以显着降低沥青混合物的制造过程中骨料和沥青的混合温度以及沥青路面的建造期间的压实温度,从而缩短了工期。它减少了能源消耗。

著录项

  • 公开/公告号KR102150381B1

    专利类型

  • 公开/公告日2020-09-01

    原文格式PDF

  • 申请/专利权人 TNTECH CO. LTD.;PARK WAN SIN;KIM CHANG GEUN;

    申请/专利号KR20200009611

  • 发明设计人 박완신;김창근;

    申请日2020-01-28

  • 分类号C04B26/26;C04B14/38;C04B20;C04B20/10;C04B24/08;C04B24/26;

  • 国家 KR

  • 入库时间 2022-08-21 11:03:54

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号