Polyaluminium chloride reduction method and manufacturing method of torrefied wood flour natural material based coagulant

机译:聚氯化铝的还原方法及木粉天然原料凝结剂的制造方法

摘要

The method for reducing polyaluminum chloride of a natural material mixture coagulant using semi-carbonized wood according to the present invention includes: S1) chipping the wood to a certain size or less using an industrial chipper; and S2) superheated steam treatment of the wood obtained after the chipping step. A step of superheated steam treatment in an apparatus, S3) inserting the superheated semi-carbonized wood chips into a crusher and pulverizing them into semi-carbonized wood powder in the range of 75 µm to 160 µm, and S4) the semi-carbonized wood powder as a synthetic weapon. It characterized in that it comprises the step of mixing with polyaluminum chloride which is a polymer coagulant.
机译:根据本发明的使用半碳化木减少天然材料混合凝结剂的聚氯化铝的方法包括:S1)使用工业削片机将木片削成一定尺寸或更小; S2)对切屑工序后得到的木材进行过热蒸汽处理。在设备中进行过热蒸汽处理的步骤,S3)将过热的半碳化木屑插入破碎机中,然后将其粉碎成75 µm至160 µm的半碳化木粉,S4)将半碳化木粉作为合成武器。其特征在于它包括与作为聚合物凝结剂的聚氯化铝混合的步骤。

著录项

获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号