摘要

FIELD: chemistry.;SUBSTANCE: invention relates to production of pipes with protective fiberglass coating, glass tape for coating of pipe, method of applying glass tape on steel pipe and device for application of glass tape on steel pipe. Pipe contains a coating from glass tape containing a cloth from glass winding impregnated with polymer me at that, the web is formed unwinding glass winding from bobbins and pulling glass-spinning through a system of shafts, which swirl threads at bending, the formed web is impregnated with polymer melt at melt temperature from 100 °C to 250 °C, as used polyethylene melt containing component A in the form of homo- and/or ethylene copolymer with density of 0.910–0.960 g/cm3, component B in the form of homo- and/or copolymer of propylene with density of 0.860–0.920 g/cm3 and a stabilizer selected from: pentaerythrol tetrakis-3-(3,5-ditertbutyl-4-hydroxyphenyl)propionate, 2,6-di-tert-butyl-para-cresol, tris(2,4-di-tert-butylphenyl)phosphite, dysteryl thiodipropionate with the following content of components: component A from 49.2 % to 89.9 %, component B from 10 % to 50 %, stabilizer from 0.1 % to 0.8 %.;EFFECT: invention provides lower rigidity of pipe for bending, reliable protection of pipe against mechanical damages during installation and operation of pipeline and longer service life of constructed pipeline.;8 cl, 3 dwg, 1 tbl
机译:技术领域本发明涉及具有保护性玻璃纤维涂层的管道的生产,用于管道涂层的玻璃带,在钢管上施加玻璃带的方法以及在钢管上施加玻璃带的装置。管子包含玻璃带的涂层,玻璃带包含一块布,玻璃布缠绕有聚合物熔体;在此过程中,纤维网形成为从线轴上解开玻璃绕制,并通过轴系统拉动玻璃纺丝,该系统在弯曲时旋转涡旋线,形成的纤维网在聚合物温度为100°C至250°C的温度下被聚合物熔体浸渍二手聚乙烯熔体,其组分A为均聚物和/或乙烯共聚物,密度为0.910-0.960 g / cm 3 ,组分B为均聚物和/或丙烯共聚物,且密度为0.860–0.920 g / cm 3 ,稳定剂选自:季戊四醇-3-(3,5-二叔丁基-4-羟基苯基)丙酸酯,2,6-二叔丁基-对甲酚,三(2,4-二叔丁基苯基)亚磷酸酯,硫代二丙酸硬脂酯,组分含量如下:组分A从49.2%至89.9%,组分B从10%至5​​0%,稳定剂从0.1%至0.8%.;效果:本发明提供了较低的弯曲刚性,可在管道安装和运行过程中可靠地保护管道免受机械损坏。人工管道的使用寿命; 8 cl,3 dwg,1 tbl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号