Polyvinylidene fluoride and Ultem(TradeMark) polyetherimide were dissolved in 50/50 acetone/N,N dimethylformamide (DMF) and 80/20 tetrahydrofuran/DMF, respectively, and electrospun. Polymer solution concentrations and molecular weights were changed while other spinning parameters (voltage, distance, solution feed rate) were held constant. Fiber diameters in the resulting electrospun mats varied from 0.25 to 4.4 microns, increasing with polymer concentration and molecular weight; trends in diameter were compared with trends in viscosities and surface tensions of the spinning solutions.