Development of a Co-free NdFeB anisotropic bonded magnet produced from the d-HDDR processed powder

机译:

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

The NdFeB anisotropic bonded magnet produced by the HDDR method, which was developed in 1990, has not found general popularity due to its high cost and low serviceable temperature of 353 K. The authors have developed a new production method that overcomes these barriers to decrease the cost and increase the serviceable temperature. The use of the dynamic HDDR (d-HDDR) process eliminates the need for Co, thus greatly reducing the production cost of NdFeB anisotropic bonded magnets with a (BH)max of 159 kJ/m{sup}3 - The anisotropy of the NdFeB magnetic powder is induced by the control of the reaction rate of the NdFeB alloy and hydrogen, by controlling the hydrogen pressure in the HDDR process. The serviceable temperature is increased by the addition of Dy after the application of the d-HDDR method. An increase in intrinsic coercivity, iHc, from 1.12 MA/m to 1.56 MA/m, corresponds to a proportional increase in the serviceable temperature to 413 K.

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号