The present paper describes the quality and its improvement of friction welded joints between a rectangular section bar and a circular section bar. Three kinds of rectangular section bars with different aspect ratio were used for the experiment. The rectangular section bars and circular section bars were joined by using a continuous drive (brake type) friction welding machine with an electromagnetic clutch in order to prevent a braking deformation during rotation stop. The low heat input friction welding method (LHI method) was used for joining. The following conclusions were given. (l)The first phase of the friction stage was composed of wear and seizure stages. This result was similar to the join of circular section bars of same diameter. (2)When the areas of the weld faying surfaces were same each other, the initial torque and the elapsed time for initial torque hardly changed in spite of the aspect ratios of rectangular section bars. (3)The welded joints obtained only the first stage (up to initial torque) had 100 percent joint efficiency, but fractures occurred between the welded interface and base metal. When small aspect ratios of rectangular section bars and a circular section bar were welded, several joints fractured at the base metal although they had a little defect in the welded interface. (4)When the joints were made by the LHI method in Ar atmosphere, the welded joints had 100 percent joint efficiency, but fractures occurred between the welded interface and base metal. (5)The welded joints had 100 percent joint efficiency and fractured at the base metal when the joints were made by the LHI method with adding forge pressure (improving LHI method). On the other hand, most of the welded joints made by the conventional method with forge pressure had fractures occurred between the welded interface and base metal. (6)The improving LHI method has more advantages than those welded by the conventional method, i.e., less burn-off, less burr and less deformation of welded interface area. As a conclusion, it was clarified that the improving LHI method is the most effective friction welding method for rectangular section bars and circular section bars.
机译:本文介绍了矩形型材和圆形型材之间的摩擦焊接接头的质量及其改进。实验采用3种不同纵横比的矩形截面条。矩形截面钢筋和圆形截面钢采用带电磁离合器的连续驱动(制动式)摩擦焊机连接,以防止旋转停止时制动变形。采用低热输入摩擦焊接法(LHI法)进行连接。得出以下结论。(l)摩擦阶段的第一阶段由磨损和卡住阶段组成。该结果类似于相同直径的圆形截面棒的连接。(2)当焊缝褪色面的面积彼此相同时,尽管矩形截面的纵横比不同,但初始扭矩和初始扭矩的经过时间几乎没有变化。(3)仅获得第一级(最高初始扭矩)的焊接接头具有100%的接头效率,但焊接界面和母材之间发生了断裂。当焊接矩形截面棒和圆形截面棒的小纵横比时,尽管它们在焊接界面上有一点缺陷,但几个接头在母材处断裂。(4)在Ar气氛下采用LHI法制作接头时,焊接接头的接头效率为100%,但焊接界面与母材之间发生断裂。(5)焊接接头具有100%的接头效率,并且当通过LHI方法加锻压力(改进LHI方法)进行接头时,在母材处断裂。另一方面,大多数采用锻造压力方法制成的焊接接头在焊接界面和母材之间都发生了断裂。(6)改进的LHI方法比传统方法焊接的LHI方法具有更多的优点,即烧掉更少,毛刺更少,焊接界面面积变形更少。综上所述,改进LHI法是矩形截面钢筋和圆形截面钢材最有效的摩擦焊接方法。

著录项

相似文献

  • 外文文献
  • 中文文献
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号