Energy deposition at front and rear surfaces during picosecond laser interaction with fused silica

机译:Energy deposition at front and rear surfaces during picosecond laser interaction with fused silica

获取原文
获取原文并翻译 | 示例
           

摘要

The difference between front-surface and rear-surface energy deposition of a 35 ps laser pulse (λ=1064 nm) in fused silica was investigated using shadowgraphic and laser-deflection techniques. Shock waves were observed in the glass and in air. Shock waves generated in air at the front surface are stronger than at the rear surface. Less than 35 of the energy incident on the surface drives the air shock waves at the rear surface. Up to 90 of the incident energy drives the air shock waves at the front surface. Laser-plasma interaction is responsible for this difference and for limiting the amount of energy deposited inside the sample during front-surface ablation. Energy deposition at the rear surface is mostly limited by self-focusing inside the material.

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号