Three-dimensional (3-D) tomographic images of a nodular graphite cast iron obtained using a laboratory X-ray source were used to analyze the opening of a fatigue crack during in situ mechanical loading. Direct image analysis and digital image correlation are utilized to obtain the 3-D morphology and front location of the crack, as well as the displacement fields in the bulk of the specimen. From digital image correlation results it is possible to extract the crack opening displacement (COD) map in the whole sample cross-section and to compute stress intensity factors (SIFs) all along the crack front, even for COD values that are less than the image resolution. The comparison of COD maps with local values of the SIF enabled for an estimation of the opening SIF (K_(op)) equal to 6 MPa m~(1/2).
机译:使用实验室 X 射线源获得的球墨铸铁的三维 (3-D) 断层扫描图像用于分析原位机械载荷期间疲劳裂纹的打开。利用直接图像分析和数字图像相关来获得裂纹的三维形貌和前沿位置,以及大部分试样的位移场。从数字图像相关结果中,可以提取整个样品横截面中的裂纹张开位移 (COD) 图,并计算整个裂纹前沿的应力强度因子 (SIF),即使 COD 值小于图像分辨率也是如此。将COD图与SIF的局部值进行比较,可以估计等于6 MPa m~(1/2)的开口SIF(K_(op))。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号