Abstract:Endothelial cell adherence to uncoated gelatin‐impregnated Dacron (Gelseal) is poor but can be significantly improved by precoating with a suitable basement membrane such as fibronectin. To assess the suitability of fibronectin‐coated Gelseal for endothelial cell seeding, fibronectin binding to Gelseal and its dissociation kinetics were investigated. Fibronectin binding was quantified by radiolabeling human fibronectin with iodine 125, concentrations of 10, 25, 50, 150, and 250 γg/ml being used to coat Gelseal at 30, 60, and 90 min of incubation. The amount of fibronectin bound was directly proportional to the concentration used and increased with time of incubation (p<0.05). However, the percentage attachment decreased with increasing concentration (p<0.001). The number of molecules bound per centimeter squared of graft was calculated. In the first 30 min, 75 of bound fibronectin was lost after exposure to a flow rate of 200 ml/min in a pulsatile artificial circulation; thereafter, the fibronectin‐Gelseal bond was stable for up
机译:摘要:内皮细胞对未包被明胶浸渍的涤纶(Gelseal)的粘附性较差,但用合适的基底膜(如纤连蛋白)预包可以显著改善。为了评估纤连蛋白包被的 Gelseal 对内皮细胞接种的适用性,研究了纤连蛋白与 Gelseal 的结合及其解离动力学。通过用碘 125 放射性标记人纤连蛋白来定量纤连蛋白结合,碘 125 浓度为 10、25、50、150 和 250 γg/ml,用于在孵育 30、60 和 90 分钟时包被 Gelseal。纤连蛋白结合的量与使用的浓度成正比,并随着孵育时间的增加而增加(p<0.05)。然而,随着浓度的增加,附着率下降(p<0.001)。计算每平方厘米移植物结合的分子数。在前 30 分钟内,在脉动人工循环中暴露于 200 ml/min 的流速后,75% 的结合纤连蛋白丢失;此后,纤连蛋白-Gelseal 键稳定 up

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号