Zinc oxide (ZnO) and titanium dioxide (TiO2) nanoparticles (NPs) were biosynthesized by using aloe vera extract for tunable Q-switched application. ZnO TiO2 NPs was then prepared as a saturable absorber (SA) via mechanical exfoliation technique. By measuring nonlinear optical absorption, the modulation depth and satu-ration intensity were 1.57 and 0.05 MW/cm2, respectively. The obtained output pulse had a 1567.60 nm central wavelength and a signal-to-noise ratio (SNR) of 44.94 dB at a pump power of 248.50 mW. The increase of pump power from 178.00 mW to 248.50 mW has led to continuously increase in the repetition rate from 7.70 kHz to 12.99 kHz and decrease from 45.35 mu s to 28.93 mu s of pulse width, respectively. At maximum pump power, 5.06 nJ of pulse energy was also recorded. When the tunable bandpass filter (TBF) was incorporated into the cavity, the wavelength-tunable Q-switched pulses was constructed, and the tuning wavelength from 1530 nm to 1570 nm that of 40 nm covering wavelength was attained. This finding suggests that a wider range of tunable and simple designs is applicable to optical communications and sensing applications.
机译:利用芦荟提取物生物合成氧化锌(ZnO)和二氧化钛(TiO2)纳米颗粒(NPs),用于调Q开关应用。然后通过机械剥离技术制备了ZnO TiO2 NPs作为饱和吸收剂(SA)。通过测量非线性光吸收,调制深度和饱和比强度分别为1.57 %和0.05 MW/cm2。得到的输出脉冲的中心波长为1567.60 nm,信噪比(SNR)为44.94 dB,泵浦功率为248.50 mW。泵浦功率从178.00 mW增加到248.50 mW,导致重复频率从7.70 kHz持续增加到12.99 kHz,脉冲宽度从45.35 μ s下降到28.93 μ s。在最大泵浦功率下,还记录了 5.06 nJ 的脉冲能量。当将可调谐带通滤光片(TBF)掺入腔体中时,构建了波长可调的调Q脉冲,并实现了从1530 nm到1570 nm的调谐波长,即40 nm覆盖波长。这一发现表明,更广泛的可调谐和简单设计适用于光通信和传感应用。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号