Atomistic Mechanism of the Nucleation of Methylammonium Lead Iodide Perovskite from Solution

机译:甲基铵碘化铅钙钛矿从溶液中成核的原子机理

获取原文
获取原文并翻译 | 示例
获取外文期刊封面目录资料

摘要

In the ongoing intense quest to increase the performance of perovskite solar cells, optimizing the morphology of perovskite material has become imperative to achieve high power conversion efficiencies. Despite the fact that nucleation plays a key role in controlling the crystal morphology, very little is known about the nucleation and crystal growth processes. Here, we perform metadynamics simulations of nucleation of methylammonium lead triiodide (MAPI) in order to unravel the atomistic details of perovskite crystallization from a gamma-butyrolactone solution. The metadynamics trajectories show that the nucleation process takes place in several stages. Initially, dense amorphous clusters mainly consisting of lead and iodide appear from the homogeneous solution. These clusters evolve into lead iodide (PbI2)-like structures. Subsequently, methylammonium (MA(+)) ions diffuse into these PbI2-like aggregates triggering the transformation into a perovskite crystal through a solid solid transformation. These enticing results allowed us to design new experimental strategies to rationally control the dimensions of MAPI grains using the spin-coating technique and to engineer homogeneous nucleation and growth of MAPI single crystals. The experimental results amply support our unprecedented observations related to the critical role of monovalent cations in inducing the nucleation process in lead halide perovskites.
机译:在不断追求提高钙钛矿太阳能电池性能的过程中,优化钙钛矿材料的形貌已成为实现高功率转换效率的必要条件。尽管成核在控制晶体形态方面起着关键作用,但人们对成核和晶体生长过程知之甚少。在这里,我们对甲基三碘化铅铵(MAPI)的成核进行了元动力学模拟,以揭示γ-丁内酯溶液中钙钛矿结晶的原子细节。元动力学轨迹表明,成核过程分几个阶段进行。最初,主要由铅和碘化物组成的致密无定形团簇从均相溶液中出现。这些团簇演变成碘化铅(PbI2)样结构。随后,甲基铵 (MA(+)) 离子扩散到这些 PbI2 样聚集体中,通过固体转变触发转化为钙钛矿晶体。这些诱人的结果使我们能够设计新的实验策略,使用旋涂技术合理控制MAPI晶粒的尺寸,并设计MAPI单晶的均匀成核和生长。实验结果充分支持了我们前所未有的观察结果,即一价阳离子在诱导卤化铅钙钛矿成核过程中的关键作用。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号