The present study focused on the mechanical properties of stir cast Al 6063/Al_(2)O_(3)(alumina) reinforced metal matrix composites. Aluminum-alumina composites are used in various industries including fabrication, aerospace, automobile sectors, etc. The properties like corrosion resistance, low density, and high modulus of elasticity, higher thermal, and electrical conductivity make them the best choice for its applications in various industries (Prasad, 2004). The present work focus on the hardness of Al 6063/Al_(2)O_(3)(alumina) reinforced metal matrix composites by varying the percentage of the reinforced element alumina in the base matrix alloy Al 6063, stirring speed and stirring time (Kok, 2005). The thickness of the sample was taken 10 mm, width 30 mm and length 100 mm. Nine samples were prepared by varying the percentage of alumina 2, 4, 6 (wt ), stirring speed of 800, 1000 and 1200 (Rpm) and stirring time of 5, 10, 15 (minutes). In this experiment work various works has been reviewed in which lower concentration of alumina was taken to analyse the effect on the response factor, that's why lower even concentration of alumina was taken. It was shown from the experiment that the hardness value increases with the increase in reinforcement percentage but after that, there was a decrease in hardness value.
机译:本研究主要研究了搅拌铸造Al 6063/Al_(2)O_(3)(氧化铝)增强金属基复合材料的力学性能。铝铝复合材料用于各种行业,包括制造、航空航天、汽车行业等。耐腐蚀性、低密度、高弹性模量、更高的导热性和导电性等特性使其成为各种行业应用的最佳选择(Prasad,2004 年)。本研究的重点是通过改变基础基体合金Al 6063中增强元素氧化铝的百分比、搅拌速度和搅拌时间来研究Al 6063/Al_(2)O_(3)(氧化铝)增强金属基复合材料的硬度(Kok,2005)。样品的厚度为10毫米,宽度为30毫米,长度为100毫米。通过改变氧化铝的百分比2%、4%、6%(wt %),搅拌速度为800、1000和1200(Rpm),搅拌时间为5、10、15(分钟)制备了9个样品。在这项实验工作中,已经回顾了各种工作,其中采用了较低浓度的氧化铝来分析对响应因子的影响,这就是采用较低浓度氧化铝的原因。实验表明,硬度值随增强率的增加而增加,但之后硬度值下降。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号