首页> 外文期刊>Catalysis science & technology >Au/Co promoted CeO2 catalysts for formaldehyde total oxidation at ambient temperature: role of oxygen vacancies
【24h】

Au/Co promoted CeO2 catalysts for formaldehyde total oxidation at ambient temperature: role of oxygen vacancies

机译:非盟/公司促进了CeO2甲醛的催化剂总氧化在环境温度:角色氧空位

获取原文
获取原文并翻译 | 示例
           

摘要

Au catalysts with loadings of 1.5 and 3 wt% were dispersed over CeO2 and Co (9; 12 mol%) promoted CeO2, using the deposition-precipitation method, followed by calcination at 350 degrees C. The fresh supported Au catalysts were characterized using several techniques in order to investigate their morphological, structural and redox properties before being tested for formaldehyde (HCHO) total oxidation. All of the supported Au catalysts exhibited HCHO oxidation into CO2 at 25 degrees C and demonstrated a great stability for the time on stream (40 h). The 3 wt% Au catalysts demonstrated a higher HCHO conversion than their low-gold counterparts (1.5 wt% Au), a remarkable improvement in the HCHO conversion was observed using Co-promoted ceria (9 mol%). Based on the HCHO amount (in mu mol) converted into CO2 per gram of gold per second after 40 h on stream, the 1.5Au/CeCo catalyst demonstrated the best activity (similar to 3.9) as compared to the other catalysts (<= 2.0). X-ray photoelectron spectroscopy (XPS) characterization of the fresh catalysts indicated that the Au species were mainly in a slightly ionic delta(+) valence state, but did not exclude the possibility of metallic gold. Furthermore, no marked changes were found in gold dispersion upon adding cobalt. Promotion of the HCHO oxidation over gold supported on Co-promoted ceria catalysts can be related to the higher concentration of oxygen vacancies and an improvement in the redox properties, which can contribute to the better activation of O-2 and an enhancement of the oxygen mobility.
机译:非盟催化剂载荷为1.5和3 wt %分散在CeO2和有限公司(9;CeO2,使用deposition-precipitation方法,其次是在350度c .煅烧新鲜催化剂支持非盟进行表征使用一些技术来调查他们的形态,结构和氧化还原属性进行甲醛检测之前总氧化(一氧化碳)。催化剂表现出一氧化碳氧化成二氧化碳在25岁度,并演示了一个伟大的稳定时间在流(40小时),3 wt %盟催化剂演示了一个一氧化碳转化率比他们的高low-gold同行(1.5 wt % Au),一个了不起的改善一氧化碳转换观察使用Co-promoted二氧化铈(9摩尔%)。一氧化碳量(μ摩尔)转化成二氧化碳/克黄金每秒40小时后流,1.5 au / CeCo展示最好的催化剂活动(类似于3.9)相比其他催化剂(< = 2.0)。能谱(XPS)表征的新鲜催化剂表示,非盟物种主要在稍微δ(+)离子价状态,但不排除的可能性金属黄金。被发现在黄金分散添加钴。促进一氧化碳氧化超过黄金支持Co-promoted二氧化铈催化剂与氧气的浓度更高职位空缺,改善氧化还原属性,可以导致更好的激活0 2和一个增强的氧气流动。

著录项

相似文献

  • 外文文献
  • 中文文献
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号