...
首页> 外文期刊>Spectrochimica acta, Part A. Molecular and biomolecular spectroscopy >Molecular structure characterization of bituminous coal in Northern China via XRD, Raman and FTIR spectroscopy
【24h】

Molecular structure characterization of bituminous coal in Northern China via XRD, Raman and FTIR spectroscopy

机译:XRD,拉曼和FTIR光谱法中北方沥青煤的分子结构特征

获取原文
获取原文并翻译 | 示例

摘要

Bituminous coal is used widely for a variety of applications despite causing a range of problems within processes. The complexity and heterogeneity of the molecular structure of coal is one of the reasons for problems during use. Investigation into the molecular structure of the bituminous coal is reported from using X-ray diffraction (XRD), Raman spectroscopy, and Fourier Transform infrared (FTIR) spectroscopy experiments on four coal samples from coal mines in Northern China. The average lateral sizes (L-a), stacking heights (L-c) and interlayer spacing (d(002)) of the coal samples' crystallite structures derived from the XRD ranged from 25.78 to 27.93 angstrom, 17.27 to 25.88 angstrom and 3.40 to 3.52 angstrom, respectively; and the G D-1, I-D1/I-G and L-a of the samples ranged from 245.06 to 249.63 cm(-1), 2.18 to 2.48 and 18.16 to 20.64 angstrom, respectively. The FTIR spectra reveals that coal samples incorporate oxygen-containing functional groups, aliphatic functional groups, aromatic functional groups and hydroxyl functional groups. Results show these four coal samples contained a low degree of ordered microcrystalline units with a low degree of aromatic conformation. The samples have the largest proportion of oxygenated functional groups, followed by aromatic structures, aliphatic structures and hydroxyl groups. Results from this study could inform the ongoing study of molecular structural characteristics of bituminous coal as well as help our understanding of properties such as wettability and pore structure. (C) 2021 Elsevier B.V. All rights reserved.
机译:烟煤被广泛用于各种应用,尽管在工艺过程中会造成一系列问题。煤分子结构的复杂性和非均质性是使用过程中出现问题的原因之一。利用X射线衍射(XRD)、拉曼光谱和傅里叶变换红外光谱(FTIR)对中国北方四个煤矿的煤样进行了研究。由XRD得到的煤样微晶结构的平均横向尺寸(L-a)、堆积高度(L-c)和层间间距(d(002))分别为25.78至27.93埃、17.27至25.88埃和3.40至3.52埃;样本的GD-1、I-D1/I-G和L-a分别为245.06至249.63厘米(-1)、2.18至2.48和18.16至20.64埃。FTIR光谱表明,煤样中含有含氧官能团、脂肪族官能团、芳香族官能团和羟基官能团。结果表明,这四个煤样含有低程度的有序微晶单元,芳香构象低。样品中含氧官能团的比例最大,其次是芳香结构、脂肪族结构和羟基。这项研究的结果可以为正在进行的烟煤分子结构特征的研究提供信息,也有助于我们理解润湿性和孔隙结构等性质。(c)2021爱思唯尔B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号