Regeneration of waste rolling oil via inorganic flocculation-adsorption process

机译:通过无机絮凝剂吸附过程再生废油 - 吸附过程

获取原文
获取原文并翻译 | 示例
           

摘要

Waste rolling oil (WRO) can be regenerated by inorganic flocculation-adsorption. Ferric hydroxide (Fe(OH)_3) colloid prepared by the double decomposition reaction of FeCI_3 and NaOH was selected as an inorganic flocculant. Fly ash, activated carbon, clay and silica gel were used as adsorbents to treat the WRO. Effects of different treatment conditions on the performance of the recycled oil were investigated. Results indicated that the recycled oil achieved optimum quality under the following conditions: flocculation time, 6min; temperature, 60 °C; adsorption time, 20 min; and mass ratios of FeCI_3-to-WRO, NaOH-to-FeCI_3 and fly ash-to-WRO of 0.10, 3 and 0.03, respectively. NaOH combined with Fe(OH)_3 effectively removed most macromolecular impurities, organic acids, lipids, and alcohols. Fly ash exerted the best adsorption rate and adsorption effect. In addition, physicochemical properties of the recycled oils were close to those of fresh oil.
机译:废轧制油(WRO)可以通过无机絮凝吸附再生。选用FeCI_3与NaOH复分解反应制备的氢氧化铁(Fe(OH)3)胶体作为无机絮凝剂。采用粉煤灰、活性炭、粘土和硅胶作为吸附剂处理WRO。研究了不同处理条件对再生油性能的影响。结果表明,在絮凝时间为6min的条件下,再生油的质量达到最佳;温度,60摄氏度;吸附时间20min;FeCl_3与WRO、NaOH与FeCl_3和飞灰与WRO的质量比分别为0.10、3和0.03。NaOH与Fe(OH)3的结合有效地去除了大部分大分子杂质、有机酸、脂质和醇。粉煤灰的吸附速率和吸附效果最好。此外,再生油的理化性质与新鲜油相近。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号