In the present study, the laser cladding of Al2O3 on the top surface of air plasma sprayed (APSed) yttria stabilized zirconia (YSZ) coatings was carried out to improve the hot corrosion resistance of the thermal barrier coatings (TBCs) in the presence of molten salts. The coatings with and without laser cladding were subjected to a hot corrosion test at 1000 degrees C for 30 h in which a mixture of 55 wt% V2O5 and 45 wt% Na2SO4 was used as the corrosive salt. SEM micrographs and EDS analysis confirmed the formation of YVO4 rod-shaped crystals dispersed on the surface of the APSed YSZ coatings after hot corrosion test, while these crystals were hardly detected in the laser clad coatings. The SEM micrograph of the cross section of the APSed YSZ coatings revealed cracks and a thermally grown oxide (TGO) layer in the bond coat/top coat interface, which led to the complete delamination of the coatings. Supporting the SEM micrographs, XRD patterns indicated the transformation of metastable tetragonal zirconia (t-ZrO2) to monoclinic zirconia (m-ZrO2) after hot corrosion test. This structural transformation was due to the reaction of the molten salts with Y2O3 (zirconia stabilizer) which destabilized the t-ZrO2. To compare the hot corrosion resistance of the APSed YSZ and the laser clad coating, the volume percentage of the undesirable m-ZrO2 was then calculated after the hot corrosion test. This calculation revealed a higher amount of m-ZrO2 in YSZ (about 70 vol%) compared to that of the laser clad coating (about 13 vol%). (C) 2016 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
机译:在本研究中,进行Al2O3在喷涂的空气等离子体上的顶表面(APSED)ytTria稳定的氧化锆(YSZ)涂层上的激光覆层,以改善熔化存在的热阻挡涂层(TBC)的热腐蚀性盐。在1000℃下进行具有和不具有激光熔覆的涂层30小时,其中使用55wt%V2O5和45wt%Na 2 SO 4的混合物作为腐蚀性盐。 SEM显微照片和EDS分析证实了在热腐蚀试验后分散在APSED YSZ涂层表面上的YVO4棒状晶体的形成,而在激光涂层中几乎不检测到这些晶体。 APSED YSZ涂层的横截面的SEM显微照片揭示了粘合涂层/顶层涂层界面中的裂缝和热生长的氧化物(TGO)层,其导致涂层的完全分层。支持SEM显微照片,XRD图案表明,在热腐蚀试验后,将亚丙戊烷氧化锆(T-ZrO2)转化为单斜氧化锆(M-ZrO2)。这种结构转化是由于熔融盐与Y2O3(氧化锆稳定剂)的反应,其破坏T- ZrO2。为了比较APSED YSZ和激光包覆涂层的热腐蚀性,然后在热腐蚀试验后计算不希望的M-ZrO2的体积百分比。与激光包覆涂层(约13体积%)相比,该计算揭示了ysz(约70体积%)的较高量的m-zrO2。 (c)2016 Elsevier Ltd和Techna Group S.R.L.版权所有。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号