Strength of through-wall electron beam welded joint for vacuum vessel of fusion reactor

机译:用于熔体反应器真空容器的通壁电子束焊接接头的强度

获取原文
获取原文并翻译 | 示例
       

摘要

A new type of welded joint for the outer wall and rib of a double-walled vacuum vessel of a fusion reactor has been developed. The joint is manufactured by through-wall electron-beam welding (TW-EBW), in which the beam is injected from the outside of the outer wall. Static and fatigue tests are carried out on one-bead-specimens under an axial load and two-bead-specimens under a bending load. The experimental results are analytically investigated by FEM. Although this joint is partially penetrated, the net yield strength of the bead is increased by the plastic constraint due to triaxial tensile stress in the weldment. This phenomenon reduces the mean equivalent stress on the bead cross section, and the gross strength of the joint is close to that of a full thickness welded joint. The fatigue-strength reduction factor for low-cycle fatigue life is a little larger than four. The calculated fatigue-crack growth rate in the joint is conservatively calculated by using the maximum stress intensity factor of the crack and the fatigue-crack growth rate given in ASME Code Section XI.
机译:已经开发出一种新型的外壁和融合反应器的双壁真空容器的肋和肋的焊接接头。该接头由通壁电子束焊接(TW-EBW)制造,其中光束从外壁的外部注入。在弯曲载荷下在轴向载荷和双珠试样下的单珠试样上进行静态和疲劳试验。通过FEM分析实验结果。虽然该接头部分穿透,但由于焊接中的三轴拉伸应力,珠子的净产量增加。这种现象降低了珠横截面上的平均等同应力,并且接头的粗大强度接近全厚度焊接接头的粗糙度。低循环疲劳寿命的疲劳强度减少因子略大于四个。通过使用ASME代码部分XI中的裂缝的最大应力强度因子和疲劳 - 裂纹的生长速度来保守关节中的计算疲劳裂纹生长速率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号