Indium and zinc extraction from an indium-bearing zinc residue were investigated using sphalerite concentrate as a reductant in sulfuric acid medium. The effects of amount of sphalerite concentrate, sulfuric acid concentration, particle size, leaching time as well as temperature were discussed. The results showed that high indium and zinc extraction yield as well as high Fe2+/Fe3+ molar ratio could be obtained by reduction leaching of zinc residue with addition of sphalerite concentrate as a reductant. The optimal leaching condition was determined as 150 g/L H2SO4, 0.95 times of theoretic amount of sphalerite concentrate for 4 hat 90 degrees C while using particles in the range of 74-58 pm. The leaching efficiencies were 94.8% of indium, 96.1% of zinc and 92.8% of iron, respectively, and a Fe2+/Fe3+ molar ratio of 7.5 in the leach solution was also obtained. The process above was a viable method that effectively extracted zinc and indium and converted Fe3+ into Fe2+ at the same time. (C) 2016 Elsevier B.V. All rights reserved.
机译:使用闪锌矿浓缩物在硫酸介质中的还原剂中研究了从携带铟锌残留物的铟和锌提取。讨论了闪锌矿浓缩物,硫酸浓度,粒度,浸出时间以及温度的影响。结果表明,通过添加锌渣作为还原剂,通过减少锌渣的浸出,可以获得高铟和锌提取产率以及高Fe2 + / Fe3 +摩尔比。最佳浸出条件确定为150g / l H 2 SO 4,在74-58μm范围内的颗粒在74-58μm的范围内使用颗粒的颗粒的0.95〜9.5倍。浸出效率分别为94.8%的铟,96.1%的锌和92.8%的铁,也得到了浸出溶液中的7.5的Fe2 + / Fe3 +摩尔比。上述方法是一种可行的方法,其在同一时间有效地将锌和铟和转化为Fe2 +的Fe2 +。 (c)2016年Elsevier B.v.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号