The catalytic membrane reactors (CMR) were prepared using commercial Hollow Fiber Membranes of corundum with 4 nm or 1400 nm pores and impregnated with palladium. The tests performed were phenol hydrogenation, hydrogen peroxide generation to oxidize phenol by advanced oxidation processes and chromium (VI) reduction. Reactions were performed in aqueous solution, at mild temperature and under atmospheric pressure. For all tests, the hydrogen passed through the membrane to be activated with palladium. The test with phenol showed that, in the absence of oxygen, the activated hydrogen reacts with the organic matter, leading to the formation of hydrogenated products; in the presence of oxygen, active hydrogen reacts with oxygen to form hydrogen peroxide and subsequently hydroxyl radicals that attack the organic matter until its mineralization. Furthermore, the CMR is capable of reducing chromium (VI) to chromium (III). The CMRs of smaller pore size presented better performance in all reactions.
机译:催化膜反应器(CMR)使用刚玉的商业中空纤维膜制备,用4nM或1400nm孔浸渍并用钯浸渍。进行的试验是苯酚氢化,过氧化氢通过晚期氧化方法和铬(VI)氧化苯酚。在水溶液中,在温和的温度下和大气压下进行反应。对于所有测试,氢通过膜通过钯活化。用苯酚的试验表明,在没有氧的情况下,活化的氢与有机物质反应,导致形成氢化产物;在氧气存在下,活性氢与氧气反应以形成过氧化氢,随后染色的羟基自由基,直至其矿化。此外,CMR能够将铬(VI)还原为铬(III)。较小的孔径的CMR在所有反应中呈现出更好的性能。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号