Lining of Aluminum Alloys with Hard-Metal Foils Using Shot Peening

机译:使用射击喷丸铝合金铝合金用硬质金属箔衬里

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

A method for lining aluminum alloys with hard-metal foils using shot peening is proposed. The foil is bondedto the surface of the aluminum alloy due to plastic deformationgenerated by the collision of the shots. The foil and base metalare heated to a temperature of 500 deg C to improve theweldability. A test using a single shot is carried out to evaluatethe possibility of bonding. In this test, aluminum alloyworkpieces are A2017 and A5056, and the hard-metal foils aremild steel, nickel, titanium and stainless steel SUS304 of 0.1mm thickness. By inserting a pure aluminum foil, the hard-metal foil is successfully bonded to the aluminum alloys, even atroom temperature. Finally, in actual shot peening using manyshots, the hard-metal foils are bonded over the surface of the base metals.
机译:提出了一种用射击喷丸用硬质金属箔衬里铝合金的方法。 由于镜头的碰撞,箔由于塑料变形而粘合到铝合金的表面上。 箔和基础金属的温度加热至500℃的温度以改善隔离性。 使用单次射击进行测试,以评估粘合的可能性。 在该试验中,铝合金工厂是A2017和A5056,硬质金属箔半钢,镍,钛和不锈钢SUS304,厚度为0.1mm。 通过插入纯铝箔,硬金属箔成功地粘合到铝合金,甚至在铝合金温度下。 最后,在使用Manyshots的实际喷丸中,硬金属箔在基础金属的表面上粘合。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号