摘要

At the heading of high4ensile bolt with work-hardend drawing wire, Bauschinger effect appears and raises the tool life. On the other hand, this effect reduces the shank strength of bolt. This paper proposes the steel which has large Bauchinger effect at the heading of drawing wire and the aging process which reduces the Bauschinger effect in the bolt shank. Mn or Si do not raise the Bauschinger effect. Carbon raises this effect and the high cooling rate after rolling of wire is useful too. Reduction of yield strength and tensile strength of bolt shank after compression are 15-17% and 6-7%, respectively. These reductions in strength are recovered by aging. It is concluded that aging at 573K recovers the reduction of yield strength and tensile strength of bolt-shank by the compression under strain no more than 0.03. During the compression of drawing wire, X-ray diffraction half value breadth which corresponds to the dislocation density indicates constant value. This fact suggests that the number of dislocations which are newly genereted under compression is nearly equal to that which distinguishes by the Bauschinger effect.
机译:在带有工作硬化拉丝的高强度螺栓的头部,出现鲍辛格效应并延长了刀具寿命。另一方面,这种效果降低了螺栓的柄强度。本文提出了一种在拉丝方向具有较大的鲍辛格效应的钢,以及时效处理可以降低螺栓杆中的鲍辛格效应的钢。 Mn或Si不会提高鲍辛格效应。碳提高了这种效果,轧制线材后的高冷却速度也很有用。压缩后螺栓柄的屈服强度和抗拉强度降低分别为15-17%和6-7%。这些强度的降低可通过老化来恢复。结论是,在不超过0.03的应变下压缩,在573K时效可以恢复螺栓柄的屈服强度和抗拉强度的降低。在拉丝的压缩过程中,与位错密度相对应的X射线衍射半值宽度表示恒定值。这一事实表明,在压缩作用下新产生的位错数几乎等于由鲍辛格效应所区分的位错数。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号