CaO-La2O3-MgO and BaO-La2O3-MgO catalysts with different compositions have been studied for their bulk and surface properties (viz. crystal phases, surface area, acidity/acid strength distribution, basicity/oase strength distribution, etc.) and catalytic activity/selectivity in the oxidative coupling of methane (OCM) at different processing conditions (reaction temperature, 700-850 degrees C; CH4/O-2 ratio in feed, 3.0, 4.0 and 8.0 and GHSV, 102000 and 204000 cm(3) g(-1) h(-1)). The surface acidity and strong basicity of La2O3-MgO are found to be increased due to the addition of a third component (CaO or BaO), depending upon its concentration in the catalyst. The addition of CaO or BaO to La2O3-MgO OCM catalyst causes a significant improvement in its performance. Both the CaO- and BaO-containing catalysts show a high activity and selectivity at 800 degrees C, whereas, the activity and selectivity of BaO-containing catalysts at 700 degrees C is lower than that of CaO-containing catalysts.
机译:研究了具有不同组成的CaO-La2O3-MgO和BaO-La2O3-MgO催化剂的体积和表面性质(即晶相,表面积,酸度/酸强度分布,碱度/绿洲强度分布等)和催化性能甲烷(OCM)在不同加工条件下(反应温度为700-850摄氏度;进料中CH4 / O-2的比例为3.0、4.0和8.0以及GHSV为102000和204000 cm)的活性/选择性g(-1)h(-1))。发现由于添加了第三种成分(CaO或BaO),La2O3-MgO的表面酸度和强碱性提高了,这取决于其在催化剂中的浓度。向La2O3-MgO OCM催化剂中添加CaO或BaO会显着改善其性能。含CaO的催化剂和含BaO的催化剂在800℃下均显示高活性和选择性,而含BaO的催化剂在700℃下的活性和选择性比含CaO的催化剂低。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号