Laboratory scale tests have been used to assess whether a loosely fitted PE liner within a rigid host pipe could, at any realistic working pressure, fail by rapid crack propagation (RCP). The standard 'S4' test method for RCP was modified, the usual cage of containment rings being replaced by a rigid, closed sleeve maintaining a predefined radial clearance from the unpressurised pipe. Pipe specimens of 125 mm diameter with wall thicknesses of 11-4 and 7-1 mm, made from a PE80 polyethylene in which RCP is normally possible at 0℃, were tested with three different clearances as well as with the usual S4 cage. For pipe having an unpressurised clearance down to 2% or so of the diameter, the RCP critical pressure was increased by ~50% for both thicknesses; for smaller clearances, by progressively more. These results reinforce suspicions that pipe installation conditions may affect full scale RCP resistance.
机译:已经使用实验室规模的测试来评估在任何实际工作压力下,在刚性主管内松散安装的PE衬里是否会因快速裂纹扩展(RCP)而失效。修改了用于RCP的标准“ S4”测试方法,用坚固的封闭式套筒代替了通常的密封圈笼,该套筒保持了与未加压管道之间的预定径向间隙。由PE80聚乙烯制成的125 mm直径,壁厚分别为11-4和7-1 mm的管样品在3个不同的间隙以及普通的S4笼中进行了测试,通常在0℃下可以进行RCP。对于无压间隙减小到直径的2%左右的管道,两种厚度的RCP临界压力都增加了约50%。对于较小的间隙,逐渐增加。这些结果使人们更加怀疑管道安装条件可能会影响满量程RCP的抵抗力。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号