Due to difficulties in determining modulus of elasticity of wood, only strain or deflection profiles caused by relaxation of internal stress are normally evaluated for industrial kiln-dried lumber. To directly assess the level of internal stress within the lumber, a new technique of measuring the restoring force on a half-split specimen has been presented and the corresponding device has been designed and constructed. Kiln-dried rubberwood specimens with dimensions of 30 or 50 mm (thickness), 130 mm (width) and 50 mm (length) were used in the study. The measured restoring force appears to vary with half-split length and specimen thickness. A mathematical model based on an elastic cantilever beam theory has been successfully developed to describe the restoring force behavior in a flexural response regime. The magnitude of the maximum linearly averaged internal stress sigma (m) can be derived without prior knowledge of the modulus of elasticity of wood. For the 30-mm-thick lumber, the derived values of sigma (m) are in general agreement with the ones obtained from the conventional McMillen slice test. Very close agreement is observed when the internal stress is at a relatively low level and its profile is approximately linear. But for the 50-mm-thick lumber, the determination of sigma (m) is less appropriate because of its relatively short flexural range. A restoring force-internal stress chart has been proposed for practical use in the lumber industry. This assessment was performed to investigate the evolution of internal stress during the conditioning and storage stages of kiln-dried rubberwood lumber.
机译:由于难以确定木材的弹性模量,因此通常仅对工业窑干木材评估由内应力松弛引起的应变或挠曲轮廓。为了直接评估木材内部的应力水平,提出了一种测量半劈裂试样上的恢复力的新技术,并设计和构造了相应的装置。在研究中使用尺寸为30或50毫米(厚度),130毫米(宽度)和50毫米(长度)的窑干橡胶木标本。测得的恢复力似乎随半裂长度和样品厚度而变化。已经成功开发了基于弹性悬臂梁理论的数学模型来描述挠曲响应状态下的恢复力行为。无需事先知道木材的弹性模量,就可以得出最大线性平均内部应力sigma(m)的大小。对于30毫米厚的木材,σ的推导值(m)与常规McMillen切片试验获得的值基本一致。当内部应力处于较低水平并且其轮廓近似线性时,观察到非常紧密的一致性。但是对于50毫米厚的木材,由于弯曲范围相对较短,因此确定σ(m)不太合适。已经提出了一种恢复力-内部应力图,可用于木材工业。进行该评估以调查窑干橡胶木木材在调理和储存阶段内应力的变化。

著录项

  • 来源
    《Wood Science and Technology》 |2016年第6期|1277-1292|共16页
  • 作者单位

    Walailak Univ, Sch Engn & Resources, Mat Sci & Engn, Thasala Dist 80160, Nakhon Si Thamm, Thailand;

    Walailak Univ, Sch Engn & Resources, Mat Sci & Engn, Thasala Dist 80160, Nakhon Si Thamm, Thailand;

    Nakhon Si Thammarat Seaboard Ind Coll, Pakpanang Dist 80140, Nakhon Si Thamm, Thailand;

    Walailak Univ, Sch Engn & Resources, Mat Sci & Engn, Thasala Dist 80160, Nakhon Si Thamm, Thailand;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号