首页> 外文期刊>木材工業 >10か月間の水中貯木処理スギ材の乾燥性
【24h】

10か月間の水中貯木処理スギ材の乾燥性

机译:雪松木的水下储存干燥性能为10个月

获取原文
获取原文并翻译 | 示例
获取外文期刊封面目录资料

摘要

Drying rate of Japanese cedar after water storage for ten months was examined using the 100℃ drying method. The purpose of this experiment is to confirm whether or not water storage of softwood has the effect to increase drying rate. Main results obtained were as follows: 1) Drying rate of sapwood samples increased by water storage for ten months. 2) However drying rate of heartwood samples did not change after water storage. The following explanation about drying property of softwood can be drawn according to these results that the drying rate for an actual size lumber through the total drying periods does not markedly increase by water storage for ten months because heartwood, which has the low drying rate, occupies larger portion than sapwood in the softwood lumber like sawed squares.%10か月水中貯木したスギ材について100℃試験により,乾燥開始後8時間までの乾燥経過を指数関数で近似したときの係数=乾燥速度減少係数を求め乾燥性を評価した。結果は以ドのようであった。1)10か"水中貯木したスギ試験材の含水率は.辺材では200%を越えていた。一方,心材では90%前後であった。これは伐採直後に材が示す含水率状態とほぼ近い。
机译:用100℃干燥法测定了日本雪松贮水10个月后的干燥速度。该实验的目的是确认软木的贮水是否具有提高干燥速率的作用。获得的主要结果如下:1)边贮存水10个月,边材样品的干燥速率增加。 2)然而,贮水后心材样品的干燥速率没有变化。根据这些结果,可以得出以下有关软木干燥性能的解释:由于干燥速率低的心材占据了十个月的水,因此在整个干燥期间,实际尺寸木材的干燥速率不会显着增加。 %10か月水中贮藏木したスギ材について100℃试験により,干燥开始后8时间までの干燥経过を指数关数で近似したときの系数=干燥速度减少系数1)10か“水中贮木したスギ试験材の复合率は。辺材では200%を越えていた。一方,心材では90%前后であった。これは伐采直后に材が示す伸长率状态とほぼ近い。

著录项

  • 来源
    《木材工業》 |2013年第7期|296-300|共5页
  • 作者单位

    東京大学大学院農学生命科学研究科;

    秋田県立大学木材高度加工研究所;

    職業能力開発総合大学校;

    建築研究所;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 jpn
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有