A porous clay heterostructure (PCH) from a Mexican clay was prepared and characterized, and its aqueous phenol and dichlorophenols (DCPs) adsorption capacities were studied using a batch equilibrium technique.The PCH displayed a surface area of 305.5 m~2/g, 37.2 A average porous diameter, and a basal space of 23.2 A.The adsorption capacity shown by the PCH for both phenol and DCPs from water (14.5 mg/g for phenol; 48.7 mg/g for 3,4-DCP; and 45.5 mg/g for 2,5-DCP) suggests that the PCH has both hydrophobic and hydrophilic characteristics, as a result of the presence of silanol and siloxane groups formed during the pillaring and calcination of the PCH.The values of maximal adsorption capacity for dichlorophenols were higher than those reported for aluminum pillared clays and some inorgano-organo clays and comparable with some ionic exchange resins.
机译:制备并表征了一种由墨西哥黏土制成的多孔黏土异质结构(PCH),并采用间歇平衡技术研究了其对苯酚和二氯苯酚(DCPs)的吸附能力,该PCH的表面积为305.5 m〜2 / g,37.2。平均孔径和23.2 A的基面空间.PCH对水中苯酚和DCP的吸附能力(苯酚为14.5 mg / g; 3,4-DCP为48.7 mg / g; 45.5 mg / g 2,5-DCP的g)表明PCH具有疏水和亲水特性,这是由于在PCH的柱化和煅烧过程中形成了硅烷醇和硅氧烷基团。二氯苯酚的最大吸附量值较高比报道的铝柱撑粘土和一些无机-有机粘土要高,并且可以与某些离子交换树脂相比。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号