Comparison of phosphorus recovery from incinerated sewage sludge ash (ISSA) and pyrolysed sewage sludge char (PSSC)

机译:从焚化的污水污泥灰(ISSA)和热解的污水污泥炭(PSSC)中回收磷的比较

获取原文
获取原文并翻译 | 示例
           

摘要

This research compares and contrasts the physical and chemical characteristics of incinerator sewage sludge ash (ISSA) and pyrolysis sewage sludge char (PSSC) for the purposes of recovering phosphorus as a P-rich fertiliser. Interest in P recovery from PSSC is likely to increase as pyrolysis is becoming viewed as a more economical method of sewage sludge thermal treatment compared to incineration. The P contents of ISSA and PSSC are 7.2-7.5% and 5.6%, respectively. Relative to the sludge, P concentrations are increased about 8-fold in ISSA, compared to roughly 3-fold in PSSC. Both PSSC and ISSA contain whitlock-ite, an unusual form of calcium phosphate, with PSSC containing more whitlockite than ISSA Acid leaching experiments indicate that a liquid/solid ratio of 10 with 30 min contact time is optimal to release PO_4-P into leachate for both ISSA and PSSC. The proportion of P extracted from PSSC is higher due to its higher whitlockite content. Heavy metals are less soluble from PSSC because they are more strongly incorporated in the particles. The results suggest there is potential for the development of a process to recover P from PSSC.
机译:这项研究比较并对比了焚化炉污水污泥灰(ISSA)和热解污水污泥炭(PSSC)的理化特性,目的是回收磷作为富磷肥料。随着热解被视为与焚烧相比更经济的污水污泥热处理方法,从PSSC中回收P的兴趣可能会增加。 ISSA和PSSC的P含量分别为7.2-7.5%和5.6%。相对于污泥,ISSA中的P浓度增加了约8倍,而PSSC中的P浓度则增加了约3倍。 PSSC和ISSA均含有辉绿石,这是一种不寻常的磷酸钙形式,PSSC含有比ISSA多的辉绿石。酸浸实验表明,液/固比为10且接触时间为30分钟是将PO_4-P释放到渗滤液中的最佳选择。 ISSA和PSSC。从PSSC中提取的P的比例较高,这是因为它的辉锰矿含量较高。重金属在PSSC中的溶解度较低,因为它们更牢固地结合在颗粒中。结果表明存在开发从PSSC回收P的方法的潜力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号