The utilization of the stream of waste secondary nickel-metal hydride (Ni-MH) and lithium-ion (Li-ion) cells, representing annually about 33% of all consumer batteries and accumulators placed on the Polish market, will soon become a big challenge for both legislators and plants dealing with the recycling of this type of hazardous waste. It is due to the fact that no company in Poland operating on the market has a complete technology for the processing of a full stream of waste chemical energy sources produced in this country. Until now, the most commonly used techniques of processing this type of waste were pyrometallurgical process. In this paper, the quantitative and qualitative characteristics of the stream of waste batteries and accumulators collected at separate collection points are presented. The results of metal recovery: caesium, lanthanum, cobalt, iron, manganese, nickel and zinc from the stream of waste Ni-MH cells, type R6 (AA), using hydrometallurgical methods are also offered. The paper demonstrates that one-stage leaching at an initial temperature of 25.0 °C, with 3 M H2SO4and at the solid to liquid ratio of s/l = 1/10, within 75 min, at a mixing speed of 500 rpm and in a strongly acidic environment should be adopted as optimal parameters for acid leaching of the paramagnetic fraction created after mechanical machining of Ni-MH battery, for which the leaching rates of individual metals were as follows: Ce - 97.7%, La - 88.7%, Co - 79.4%, Fe - 68.5%, Mn - 91.9%, Ni - 66.2% and Zn - 100%.
机译:废弃的二次镍氢(Ni-MH)和锂离子(Li-ion)电池流的利用量(占波兰市场上所有消费电池和蓄电池的每年约33%)将很快成为一个大问题。立法者和处理此类危险废物的工厂都面临挑战。正是由于这一事实,波兰市场上没有一家公司拥有处理该国生产的全部废弃化学能源的完整技术。迄今为止,处理此类废物的最常用技术是火法冶金工艺。本文介绍了在单独收集点收集的废电池和蓄电池流的定量和定性特征。还提供了使用湿法冶金从废镍氢电池(R6型,AA)中回收金属,铯,镧,钴,铁,锰,镍和锌的结果。本文证明了在75 min内以500 rpm的混合速度在初始温度25.0 C,3 M H2SO4和固液比为s / l = 1/10的条件下进行一阶段浸出。 Ni-MH电池机械加工后产生的顺磁性馏分的酸浸最佳参数应采用强酸性环境,其中个别金属的浸出率如下:Ce-97.7%,La-88.7%,Co- 79.4%,铁-68.5%,锰-91.9%,镍-66.2%和锌-100%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号