The shortage of waste landfill space for waste disposal and the high demand for fill materials for land reclamation projects in Singapore have prompted a study on the feasibility of using spent copper slag as fill material in land reclamation. The physical and geotechnical properties of the spent copper slag were first assessed by laboratory tests, including hydraulic conductivity and shear strength tests. The physical and geotechnical properties were compared with those of conventional fill materials such as sands. The potential environmental impacts associated with the use of the spent copper slag for land reclamation were also evaluated by conducting laboratory tests including pH and Eh measurements, batch-leaching tests, acid neutralization capacity determination, and monitoring of long-term dissolution of the material. The spent copper slag was slightly alkaline, with pH 8.4 at a solid : water ratio of 1:1. The batch-leaching test results show that the concentrations of the regulated heavy metals leached from the material at pH 5.0 were significantly lower than the maximum concentrations for their toxicity limits referred by US EPA's Toxicity Characteristic Leaching Procedure (TCLP). It was also found that the material is unlikely to cause significant change in the redox condition of the subsurface environment over a long-term period. In terms of physical and geotechnical properties, the spent copper slag is a good fill material. In general, the spent copper slag is suitable to be used as a fill material for land reclamation.
机译:新加坡的废物填埋场空间不足以及新加坡土地复垦项目对填充材料的需求很高,这促使人们对使用废铜渣作为填海材料的可行性进行了研究。废铜渣的物理和岩土性能首先通过实验室测试进行评估,包括水力传导率和抗剪强度测试。将其物理和岩土特性与诸如沙子的常规填充材料进行了比较。还通过进行实验室测试(包括pH和Eh测量,分批浸出测试,酸中和能力测定以及材料的长期溶解监测)来评估与将废铜渣用于土地复垦相关的潜在环境影响。废铜渣为弱碱性,固体与水的比例为1:1,pH值为8.4。批量浸出测试结果表明,在pH 5.0时从材料中浸出的受管制重金属的浓度明显低于美国EPA毒性特征浸出程序(TCLP)所指的其毒性极限的最大浓度。还发现该材料不可能长期引起地下环境的氧化还原条件的重大变化。就物理和岩土性能而言,废铜渣是一种很好的填充材料。通常,废铜渣适合用作土地开垦的填充材料。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号