Conventional TIG welding is known as its low productivity and limited weld depth in a single pass. Activating TIG welding (A-TIG) can greatly improve the penetration when compared with the conventional TIG welding. The effects of five kinds of activating fluxes with single component (NaF, CaF_2, AlF_3, NaCl or CaCl_2) on penetration, microstructure and weld mechanical properties during the TIG welding of titanium alloy Ti-6Al-4V were studied. Compared with the conventional TIG welding, the experimental results show that the fluxes can greatly improve the penetration at the same welding specifications. This is because of the constriction of anode spots and the change of surface tension grads. Among them the effect of flux NaF is the best in the weld tensile strength, and the effect of flux CaF_2 on the weld bend intension is the best. The appearance of inferior crystal grains and the structure of trident crystal grains are the main reasons that the performance of weld with fluoride is improved. These experimental results can be used as an aid for selecting suitable activating flux for titanium alloy.
机译:传统的TIG焊接以其低生产率和单程焊缝深度有限而著称。与传统的TIG焊接相比,激活TIG焊接(A-TIG)可以大大提高熔深。研究了Ti-6Al-4V钛合金TIG焊接中五种单组分活化剂(NaF,CaF_2,AlF_3,NaCl或CaCl_2)对熔深,组织和焊接力学性能的影响。与传统的TIG焊接相比,实验结果表明,在相同的焊接规格下,助焊剂可以大大提高熔深。这是由于阳极斑点的收缩和表面张力梯度的变化。其中,熔剂NaF对焊缝拉伸强度的影响最好,而熔剂CaF_2对焊缝弯曲强度的影响最好。劣质晶粒的出现和三叉戟晶粒的结构是提高氟化物焊接性能的主要原因。这些实验结果可以用来帮助选择合适的钛合金活化剂。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号