Formability limit diagram (FLD) and strain limits are determined along with mechanical properties and the same are correlated with textural characterization as a function of degree of rolling in an interstitial free (IF) steel. Around 65–70% and 85–90% hot deformation were given in austenitic region. It was found that 85–90% deformation developed strong hot band texture and the texture was dominated by {112}〈110〉 and {332}〈113〉 orientations. Hot rolled steel sheets were then cold rolled to 50%, 70%, 80% and 90%, where the perfect α-fiber and γ-fiber textures were developed at 80% cold reduction. Excellent formability was obtained by batch as well as continuous mode of annealing. The new γ-fibers were developed after annealing. It was observed that IF steel sheet has to be cold rolled between 80% and 90%. From FLD plots, it was observed that IF steel sheets were highly formable.
机译:确定可成形性极限图(FLD)和应变极限以及机械性能,并将其与无间隙(IF)钢中轧制度的函数与组织特性相关联。奥氏体区域的热变形约为65–70%和85–90%。发现85-90%的变形会形成强的热带织构,并且织构主要受{112} 〈110〉和{332} 〈113〉取向的影响。然后将热轧钢板冷轧至50%,70%,80%和90%,其中在80%的冷轧率下可形成完美的α纤维和γ纤维织构。通过分批以及连续退火方式获得了出色的可成型性。退火后,新的γ纤维被开发出来。已经观察到IF钢板必须被冷轧在80%和90%之间。从FLD图中,可以观察到IF钢板是高度可成形的。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号