Impacts of cryogenic sampling processes on iron mineral coatings in contaminated sediment

机译:低温取样工艺对污染沉积物铁矿石涂层的影响

获取原文
获取原文并翻译 | 示例
           

摘要

This study focused on comparing iron mineral coatings found in contaminated sediments from a cryogenic (Cryo Core) core versus an Anaerobic Core (collected under oxygen-free and ambient conditions). After thawing the Cryo Core in an oxygen-free glovebox, a suite of analyses was applied on sediments from both cores: pH, redox potential, X-ray fluorescence (XRF), X-ray diffraction (XRD), and field-emission scanning electron microscopy (FESEM) with energy dispersive X-ray analyzer (EDX). Among the iron minerals identified, crystalline py-rite was found throughout the Cyro Core sediment samples, which is in contrast to that observed for the Anaerobic Core. Moreover, mackinawite and greigite that were ubiquitous in the Anaerobic Core were not observed in Cryo Core samples. To better understand why the metastable minerals were not present, a freeze/thaw process was simulated on Anaerobic Core samples using a liquid-nitrogen quench with surface coatings characterized by FESEM/EDX. In these quenched samples, mackinawite was no longer observed, and in its place was pyrite. In addition, both greigite and pyrite were found to be unique morphologically after quenching. Dissolution and re-precipitation of iron sulfide coatings during the freeze/thaw process appears to affect the geochemistry of the pore water through two main mechanisms of freeze-concentration and freezing potential.
机译:本研究重点是将污染沉积物中发现的铁矿涂层与厌氧芯(在无氧和环境条件下收集)进行比较。在无氧的Glovebox中解冻Cryo核心后,将在核心的沉积物上施加一套分析:pH,氧化还原电位,X射线荧光(XRF),X射线衍射(XRD)和场排放扫描电子显微镜(FeSEM)具有能量分散X射线分析仪(EDX)。在鉴定的铁矿物中,在整个口交沉积物样品中发现了结晶Py rite,这与对厌氧芯的观察到相反。此外,在Cryo核心样品中未观察到厌氧核心普遍存在的颅内核和Greigite。为了更好地理解为什么不存在亚稳矿物,使用液氮淬火在厌氧芯样品上模拟冻融过程,其具有FESEM / EDX的表面涂层。在这些猝灭样品中,不再观察到鲭岩,并且在其位置是黄铁矿。此外,在淬火后发现格里格钛矿和黄铁矿在形态上是独特的。在冷冻/解冻过程中铁硫化铁涂层的溶解和再沉淀出现在冷冻浓度和冷冻潜力的两个主要机制中影响孔隙水的地球化学。

著录项

  • 来源
    《Science of the total environment》 |2021年第15期|142796.1-142796.9|共9页
  • 作者单位

    Department of Civil and Environmental Engineering New Jersey Institute of Tech. Newark NJ 07102 United States;

    Department of Civil and Environmental Engineering New Jersey Institute of Tech. Newark NJ 07102 United States;

    Center for Contaminant Hydrology Colorado State University Fort Collins CO 80523-1320 United States;

    Center for Contaminant Hydrology Colorado State University Fort Collins CO 80523-1320 United States;

    RichLand Consulting LLC United States;

    Savannah River National Laboratory Aiken SC 29808 United States;

    Department of Chemical and Materials Engineering New Jersey Institute of Tech. Newark NJ 07102 United States;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Cryogenic coring; Surface mineral coating characterization; XRD; FESEM; Iron sulfide coatings;

    机译:低温芯;表面矿物涂层表征;XRD;FeSem;硫化铁涂料;