NMR Analysis of Polyphosphoric Acid-modified Bitumens

机译:多磷酸改性沥青的NMR分析

获取原文
获取原文并翻译 | 示例
       

摘要

Phosphorous-31 NMR spectroscopy has been used to study the behavior of polyphosphoric acid (PPA) in bitumen. Phosphorous NMR spectra were acquired on a PPA-modifled bitumen immediately after blending, and on samples that were stored at 135℃ for different periods of time. The initial NMR spectra showed resonances characteristic of phosphorous atoms in orthophosphoric acid, and in middle and end groups of phosphate chains. However, over time the number of phosphorous atoms in the middle and end groups decreased, indicating a preference of polyphosphoric acid to revert back to the orthophosphoric acid in the presence of bitumen. The NMR data did not suggest the formation of organic phosphate esters as a result of PPA modification. Phosphorous NMR spectra were also acquired on bitumen samples modified with Elvaloy~R in which polyphosphoric acid was used as a catalyst. The data showed that over time only one type of phosphorous atom remained in the bitumen. The NMR data suggest that the PPA did not react with Elvaloy~R to form esters.
机译:磷31 NMR光谱已用于研究沥青中多磷酸(PPA)的行为。混合后立即在PPA改性沥青上以及在135℃下存储不同时间的样品上获得磷NMR光谱。最初的NMR谱图显示了正磷酸中以及磷链的中端和端基中磷原子的共振特征。然而,随着时间的流逝,中端基团和端基团中的磷原子数量减少,表明在存在沥青的情况下,多磷酸倾向于还原为正磷酸。 NMR数据未表明由于PPA改性而形成有机磷酸酯。在用Elvaloy?R改性的沥青样品中也获得了磷NMR光谱,其中使用多磷酸作为催化剂。数据表明,随着时间的流逝,沥青中仅残留一种磷原子。 NMR数据表明PPA不与Elvaloy_R反应形成酯。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号