Study on the poisoning tolerance and stability of perovskite catalysts for catalytic combustion of volatile organic compounds

机译:钙钛矿型挥发性有机化合物催化燃烧的中毒耐受性和稳定性的研究

获取原文
获取原文并翻译 | 示例

摘要

La0.8Cu0.2MnO3 and La0.8Sr0.2MnO3 perovskite catalysts were prepared by the co-precipitation method. The resistance of these catalysts to sulfur poisoning was tested via catalytic combustion of toluene. The results show that the perovskite catalysts were poisoned in the presence of SO2. In the presence of dodecyl mercaptan (C12H25SH), La0.8Sr0.2MnO3 exhibits better resistance to sulfur poisoning than La0.8Cu0.2MnO3. It was determined that the SO2 deactivation is due to the formation of CuSO4 on the catalyst surface.
机译:La 0.8 Cu 0.2 MnO 3 和La 0.8 Sr 0.2 MnO 采用共沉淀法制备了3 钙钛矿催化剂。通过甲苯的催化燃烧测试了这些催化剂对硫中毒的抵抗力。结果表明,在SO 2 存在下钙钛矿催化剂中毒。在十二烷基硫醇(C 12 H 25 SH)存在下,La 0.8 Sr 0.2 MnO 3 表现出比La 0.8 Cu 0.2 MnO 3 更好的抗硫中毒能力。可以确定SO 2 失活是由于在催化剂表面形成了CuSO 4

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号