In incineration plants, nitric oxide (NO) and oxygen (O-2) are the two major gaseous components, which degrade the mechanical properties of bag-filter media. Based on the experimental results of mass, dimension, morphology, crystallinity, fiber diameter, fiber orientation and fabric strength, changes in mechanical properties of polyphenylene sulfide (PPS) needled fabrics are related to two phenomena, i.e. the crystallization and the degradation of amorphous regions and some parts of crystalline regions. Both processes affect the fabric strength, competing with each other. The relation between strength and crystallinity is divided into two phases: (1) strength is dominated by crystallinity, and (2) strength is dependent on the defects in amorphous regions and some parts of crystalline regions. An increase in NO concentration has a potential to increase the deterioration rates of amorphous and crystalline phases but the crystallization process is unaffected. An increase in O-2 concentration leads to enhancement of both crystallization and deterioration. (c) 2006 Elsevier Ltd. All rights reserved.
机译:在焚烧厂中,一氧化二氮(NO)和氧气(O-2)是两种主要的气态成分,会降低袋滤器介质的机械性能。根据质量,尺寸,形态,结晶度,纤维直径,纤维取向和织物强度的实验结果,聚苯硫醚(PPS)针刺织物的机械性能变化与两种现象有关,即结晶和非晶区的降解和晶体区域的某些部分。这两个过程都影响织物强度,相互竞争。强度和结晶度之间的关系分为两个阶段:(1)强度主要由结晶度决定;(2)强度取决于非晶区和某些结晶区的缺陷。 NO浓度的增加有可能增加非晶相和结晶相的劣化速率,但是结晶过程不受影响。 O-2浓度的增加导致结晶度增加和劣化。 (c)2006 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号