The degradation of new thermally degradable thermosets obtained by cationic curing of mixtures of DGEBA and 6,6-dimethyl (4,8-dioxaspiro[2.5]octane-5,7-dione)

机译:通过阳离子固化DGEBA和6,6-二甲基(4,8-dioxaspiro [2.5]辛烷-5,7-二酮)混合物获得的新的可热降解的热固性材料的降解

获取原文
获取原文并翻译 | 示例
获取外文期刊封面目录资料

摘要

The thermal degradation of thermosetting materials prepared by cationic copolymerization of mixtures of different proportions of diglyci-dylether of bisphenol A (DGEBA) with 6,6-dimethyl (4,8-dioxaspiro[2.5]octane-5,7-dione) (MCP) initiated by ytterbium or lanthanum triflate or using a conventional initiator, BF_3·MEA was investigated. To study the thermal degradation, several techniques were used such as thermog-ravimetry (TGA), infrared spectroscopy (FTIR) and calorimetry (DSC) and the volatiles evolved during degradation were identified by mass spectrometry. The materials prepared possess the characteristics of thermally degradable thermosets, due to the presence of ester groups in the polymer chain, which are broken at the beginning of degradation. The degradability increased when lanthanide triflates were used in the curing, especially the ytterbium salt and when the proportion of MCP in the material increased.
机译:通过将不同比例的双酚A二糖基二醚(DGEBA)与6,6-二甲基(4,8-dioxaspiro [2.5]辛烷-5,7-二酮)(MCP)进行阳离子共聚制备的热固性材料的热降解by或三氟甲磺酸镧引发或使用常规引发剂BF_3·MEA进行了研究。为了研究热降解,使用了多种技术,例如热重分析(TGA),红外光谱(FTIR)和量热法(DSC),并通过质谱鉴定了降解过程中产生的挥发物。所制备的材料具有可热降解的热固性材料的特性,这是由于聚合物链中存在酯基,该酯基在降解开始时就断裂了。当使用镧系三氟甲磺酸酯固化时,尤其是the盐,以及当材料中MCP的比例增加时,可降解性增加。