Diode Laser Effect on Enamel Microhardness After Dental Bleaching Associated with Fluoride

机译:二极管激光对含氟牙漂白后牙釉质显微硬度的影响

获取原文
获取原文并翻译 | 示例
           

摘要

Objective: The aim of this in vitro study was to evaluate the effects of diode laser irradiation on human dental enamel treated by bleaching and acidulated phosphate fluoride gels (APF) according to microhardness analysis. Background Data: The high interest of patients for aesthetics in cosmetic dentistry has led to new bleaching materials and the development of new techniques. Materials and Methods: Sixty embedded, flattened human third molar enamel fragments were randomly assigned to three groups (n=20). Group 1 received topical application of 1.23% APF photoactivated using a diode laser. Group 2 received three applications of 35% hydrogen peroxide for 5min and was photoactivated with laser for 30s in each application. Group 3 treated the same as group 2 plus a 1.23% APF application for 1min after bleaching followed by 30s of laser irradiation. Microhardness analyses were performed before and after all the treatments. Results: Analysis of variance followed by Tukey and Student statistical t-tests (p<0.05) showed significantly higher microhardness values for group 1 after treatment. No significant differences were shown before and after treatments for groups 2 and 3. Conclusion: No change was observed in enamel microhardness after treatment with hydrogen peroxide gel photoactivated using diode laser with or without APF. There was an increase in microhardness when enamel was treated only with APF photoactivated using a laser.
机译:目的:这项体外研究的目的是根据显微硬度分析,评估二极管激光辐照对漂白和酸化的氟化磷凝胶(APF)处理的人牙釉质的影响。背景数据:患者对美容牙科美学的高度兴趣导致了新的漂白材料和新技术的发展。材料和方法:将60个包埋的扁平人类第三磨牙牙釉质碎片随机分为三组(n = 20)。第一组接受了使用二极管激光器光活化的1.23%APF的局部应用。第2组接受3次35%过氧化氢的3次施加5分钟,并在每次应用中用激光光活化30秒。第3组与第2组相同,加漂白后加入1.23%APF 1min,然后激光照射30s。在所有处理之前和之后进行显微硬度分析。结果:方差分析,接着进行Tukey和Student统计t检验(p <0.05),显示治疗后第1组的显微硬度值明显更高。对于第2组和第3组,治疗前后无明显差异。结论:在用有或没有APF的二极管激光器光活化过氧化氢凝胶处理后,牙釉质显微硬度没有变化。当仅用激光光活化的APF处理牙釉质时,显微硬度增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号