Pure tetragonal-phased Ca0.9MoO4:0.1Eu(3+) (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 mu m to 1.79 mu m, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. (C) 2018 Elsevier B.V. All rights reserved.
机译:通过在水/油(w / o)相法中进行共沉积,制备了具有不同粒径的纯四方相Ca0.9MoO4:0.1Eu(3+)(CaMoO4:Eu3 +)微晶。通过煅烧温度和煅烧时间来控制所制备样品的粒度,并且随着粒度的增加,样品的结晶度提高。研究了不同粒径的CaMoO4:Eu3 +微晶的发光特性。结果表明,CaMoO4:Eu3 +样品的发射光谱强度随着粒径的增加而增加,并且彼此密切相关。发光寿命相同。 CaMoO4:Eu3 +样品的发光寿命从0.637毫秒减少到0.447毫秒,而粒径从0.12微米增加到1.79微米。这项研究不仅提供有关CaMoO4:Eu3 +的尺寸依赖性发光特性的信息,而且还为高压电瓷材料的潜在应用提供了参考。 (C)2018 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号