The inherent stiffness of birch wood-fibres makes birch an excellent raw material in the manufacture of high bulk pulp. By a combination of chemical impregnation of birch chips and pre-heating of the chips to high temperature prior to refining, it is possible to manufacture CTMP with very high bulk using a low energy input. Trials revealed that the high pre-heating temperature lowers the energy consumption considerably. At 500 ml CSF an increase in the pre-heating temperature from 110℃ to 160℃ reduced the energy consumption by more than 40%. Despite the low energy input, the shive content remained low or was even reduced and the internal bond strength, in terms of Scott-Bond, compared favourably with Spruce CTMP. In summary, a high pre-heating temperature can be used to manufacture birch CTMP with very high bulk, at a low energy consumption.
机译:桦木纤维固有的硬度使桦木成为高松浆生产中的极佳原料。通过化学浸渍桦木片和在精制之前将木片预热至高温,可以使用低能量输入以非常高的体积制造CTMP。试验表明,较高的预热温度大大降低了能耗。在500 ml CSF下,将预热温度从110℃升高到160℃可使能耗降低40%以上。尽管能量输入较低,但与Spruce CTMP相比,以Scott-Bond表示的碎屑含量仍然较低,甚至降低,内部粘结强度也很不错。总之,可以使用较高的预热温度以较低的能耗来制造体积很大的桦木CTMP。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号